NL
Gys logo
Officiële handleiding

Gys MULTIPEARL 201-4

71 pagina's·3.8 MB·Lasapparaat·PDF·ENJA
Gys MULTIPEARL 201-4
Inhoudsopgave 21 secties POWER SUPPLY · MIG MANUAL - FIG III · MANUAL · MIG SYNERGIC - FIG III · … TonenVerbergen
Page 1 of the Gys MULTIPEARL 201-4 user manual — MIG SYNERGIC - FIG III
Pagina 1 · klik om te vergroten
Pagina 1
Gys MULTIPEARL 201-4 — POWER SUPPLY diagram (page 1)
Afb. 1

This manual contains safety and operating instructions. Read it carefully before using the device for the first time and retain for future reference. MULTIPEARL 200.2 / 200.4 XL / 201.4 are multiprocess welding machines (MMA, TIG & MIG/MAG) with Synergy Technology for MIG/MAG. They are suitable for welding steel, stainless steel and aluminium. Easy and quick to set up thanks to the Synergic mode.

POWER SUPPLY

The input current (I1eff) for use at maximum output is indicated on the device. Check that the power supply and its protection (fuse and/or circuit breaker) are compatible with the current required. The device must be placed in such way that the power socket is always accessible. Do not use extension lead with a section lower than 2.5 mm². MULTIPEARL 200.2 / 200.4 XL / 201.4 are delivered with a 16A plug CEE7-7 type. It must be connected to a power supply with earth between 110V and 230V 50/60Hz protected with a 16A circuit- breaker (32A in 110V). - If the voltage is < 85V or > 265V, the device won't turn on. - Protected against overvoltage MULTIPEARL 200.2 / 200.4 XL / 201.4 will automatically stop in case of overvoltage.

Gys MULTIPEARL 201-4 — POWER SUPPLY diagram (page 1)
Afb. 2
1. Control panel 2 - Positive Dinze connector 3 - Negative Dinze connector 4 - Polarity reversal cable 5 - Euro torch connector
6. Reel adaptor 100/200mm (200.2) or 200/300mm (200.4 XL / 201.4) 7 - Power lead (2.10 m) 8 - Quick release gas connector. 9 - ON/OFF switch

The ON/OFF switch is located at the back of the machine. Turn the switch on the "I" position to start the generator. This switch must not be turned off (to "O") while welding.

MIG MANUAL - FIG III

  • Selecting MIG manual mode Keep button 2 pushed and at the same time turn the upper knob until the display shows MIG Manual. Release button 2 to validate this selection +

MANUAL

  • Wire speed adjustment Turn the upper knob to adjust the wire speed.
Gys MULTIPEARL 201-4 — MANUAL diagram (page 1)
Afb. 3
  • Arc voltage adjustment Turn the lower knob to adjust the arc voltage.
Gys MULTIPEARL 201-4 — MANUAL diagram (page 1)
Afb. 4
  • Setting management torch in SPOT and DELAY mode
  • Keep button 3 pushed to select normal mode.
  • Keep pressing button 3 and at the same time turn the upper knob to select SPOT mode and to configure it. Adjustable between 0.5 to 5 sec. In the same way turn the lower knob to configure the DELAY mode. Adjustable between 0 to 5 sec."
Gys MULTIPEARL 201-4 — MANUAL diagram (page 1)
Afb. 5

MIG SYNERGIC - FIG III

+

Page 2 of the Gys MULTIPEARL 201-4 user manual — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG)
Pagina 2 · klik om te vergroten
Pagina 2
  • Selecting MIG Synergic mode Keep button 2 pressed and at the same time turn the upper knob until "MIG Synergic" is displayed.
Gys MULTIPEARL 201-4 — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG) diagram (page 2)
Afb. 6
  • Selecting the type of wire Keep button 2 pushed and at the same time press the lower knob to go to the wire type selection menu. Select the wire type with the upper knob.
Gys MULTIPEARL 201-4 — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG) diagram (page 2)
Afb. 7
  • Selecting the wire diameter Keep the button 2 pushed and at the same time press the lower knob to go to the wire diameter selection menu. Select the diameter with the upper knob. Then release the button 2 to validate. +
Gys MULTIPEARL 201-4 — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG) diagram (page 2)
Afb. 8

Selecting the metal thickness to weld Turn the upper knob to select the metal thickness to weld.

Gys MULTIPEARL 201-4 — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG) diagram (page 2)
Afb. 9
  • Selecting the arc length Turn the lower knob to select the arc length. It gets longer (0 -> +9) or shorter (0 -> -9) enabling to more or less penetrate the metal. If you weld for the first time we recommend to set the arc length to 0.
Gys MULTIPEARL 201-4 — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG) diagram (page 2)
Afb. 10
  • Selecting the welding position Keep button 1 pushed and turn both knobs to select the welding position.
Gys MULTIPEARL 201-4 — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG) diagram (page 2)
Afb. 11
  • Setting the management torch SPOT and DELAY mode
  • Press button 3 repeatedly to select Normal mode.
  • Still pressing the button 3, turn the upper knob to get to the SPOT mode. Adjsutable between 0.5 to 5 sec. In the same way turn the lower knob to configure the DELAY mode. Adjustable between 0 to 5 sec.
Gys MULTIPEARL 201-4 — SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG) diagram (page 2)
Afb. 12

SEMI-AUTOMATIC STEEL / STAINLESS STEEL WELDING (MAG)

The device is suitable for welding 0.6/0.8/1.0 steel wire and 0.8/1.0 stainless steel wire. The device is delivered with contact tip, roller groove, liner and a torch set up for 0.8 steel or stainless steel wire. For welding 0.6 wire use a torch no longer than 3m. To change the contact tip (see fig II A). The roller is reversible 0.6/0.8. The indication on the visible

Show 4 more labels / short text on this page
+ · + · + · +
Page 3 of the Gys MULTIPEARL 201-4 user manual — PROCEDURE FOR CHANGING REELS AND TORCH ASSEMBLY (FIG IV)
Pagina 3 · klik om te vergroten
Pagina 3

side of the roller is the diameter in use. For a 0.6 wire use the 0.6 groove. Welding Steel or Stainless Steel requires using a specific gas mix - Argon + CO2 (Ar + CO2). The proportion of CO2 will vary depending on application. The gas flow for steel welding is between 8 and 12 L/min depending on the environment and experience of the welder. For specific requirements seek advice from your gas distributor. For polarity see page 4.

SEMI-AUTOMATIC ALUMINIUM WELDING (MIG)

This welding machine is suitable for welding 0.8 and 1mm aluminium wires . To weld aluminium, neutral gas “Pure Argon” (AR) is required. For choosing gas, ask a gas distributor for advice. The gas flow for welding aluminium is between 15 and 25 L/min depending on the environment and experience of the welder. Machine set-up for aluminium welding: - Use specific rollers for Aluminium - Set the pressure on the rollers to the minimum to avoid pinching the wire. - Remove the capillary tube before connecting the aluminium torch with a teflon liner. - When welding aluminium use a special aluminium torch with Teflon liner to reduce friction. Do not cut the liner near the connector! It is used to guide the wire from the rollers. (Fig II B) - Contact Tip: Use a SPECIAL aluminium contact tip corresponding to the diameter of the wire. For polarity see page 4.

"NO GAS" WELDING

To set up the machine for "No Gas" see the instructions on page 4. Welding cored wire with a standard nozzle can overheating and damage the torch. Use a nozzle special "No Gas" (ref. 041868) or remove the original nozzle (Fig III D). For polarity see page 4.

PROCEDURE FOR CHANGING REELS AND TORCH ASSEMBLY (FIG IV)

  • Remove the nozzle from the torch (fig E) and the contact tip (fig D).
  • Open the machine's side door.
  • Place the reel on the driving pin (fig A) of the reel support. For a 200mm wire reel tighten the reel to the maximum. The adaptor (1) is only to be used for a 200mm reel.
  • Adjust the reel brake (2) to avoid the reel inertia tangling the wire when welding stops. In general, do not over-tighten! Then screw in the reel support (3).
  • Fit the roller(s) suitable for your application. The rollers supplied are double grooved rollers (0.6/0.8). The indication on the visible side of the roller is the diameter in use. For a 0.8 wire, use the 0.8 groove. For Aluminium or cored wire welding use the appropriate rollers (fig B) To adjust the roller tension (fig C), process is as follows: loosen the tensioner to the maximum (4), start the motor by pressing the torch trigger, tighten the tensioner whilst pressing the trigger. Bend the wire where it comes out of the nozzle and hold it in place to stop its progress. The pressure adjustment is ideal when the guide roller slides over the wire even when it is blocked at the end of the torch. NB: for aluminium wire set the tension to the minimum not to pinch the wire.
  • Adjust the wire so 5cm protrudes from the torch then fit the contact tip (correct tip for the wire) (fig D) and the nozzle (fig E).

GAS CONNECTION The device is designed with a quick release gas connection. Use the adaptor supplied with the machine.

Gys MULTIPEARL 201-4 — PROCEDURE FOR CHANGING REELS AND TORCH ASSEMBLY (FIG IV) diagram (page 3)
Afb. 13

Type of wire FE FE ALG 5 SS FC CuSi 3 CuSi 8 CuAL ALSi 5 ALSi 12

Process MAG MAG MIG MAG MAG MIG

0.6 - 0.8 - 1.0 0.8 - 1.0 0.8 - 1.0 0.9 -1.2 0.8 0.8 - 1.0 0.8 1.0 1.0

Welding position All Flat Flat Flat All All

Page 4 of the Gys MULTIPEARL 201-4 user manual — TIG PRO (EURO TORCH)
Pagina 4 · klik om te vergroten
Pagina 4

MMA

  • Selecting MMA mode Keep button 2 pressed and at the same time turn the upper knob to select MMA mode.
Gys MULTIPEARL 201-4 — MMA diagram (page 4)
Afb. 14
  • Welding current adjustment Turn the upper knob to select the welding current.
Gys MULTIPEARL 201-4 — MMA diagram (page 4)
Afb. 15
  • Arc Force adjustment Turn the lower knob to adjust the Arc Force. Adjustable from 0 to 100%
Gys MULTIPEARL 201-4 — MMA diagram (page 4)
Afb. 16
  • Hot Start adjustment Keep pressing button 3 and at the same time turn the upper knob to adjust the Hot Start. Adjustable from 0 to 100% +
Gys MULTIPEARL 201-4 — MMA diagram (page 4)
Afb. 17

ELECTRODE WELDING

  • The reverse polarity cable must be disconnected in MMA (stick welding) mode in order to connect the electrode holder and earth clamp. Connect the electrode holder and earth clamp as indicated on the electrode packaging.
  • Respect the basic rules of welding
  • This device has 3 features specific to Inverter machines : - Hot Start: Increases the current to assist the initial striking of the arc. - Arc Force: A ponctual increase of current avoiding the electrode to be stuck in the welding pool. - Anti-Sticking: Enables easy removal of the electrode from the metal.

TIG PRO (EURO TORCH)

  • Selecting TIG Pro mode (Euro torch) Keep button 2 pushed and at the same time turn the upper knob until «TIG Pro» is displayed.
Gys MULTIPEARL 201-4 — TIG PRO (EURO TORCH) diagram (page 4)
Afb. 18
  • Welding current adjustment Use the upper knob.
Gys MULTIPEARL 201-4 — TIG PRO (EURO TORCH) diagram (page 4)
Afb. 19

+ · +

Page 5 of the Gys MULTIPEARL 201-4 user manual — TIG LIFT WELDING
Pagina 5 · klik om te vergroten
Pagina 5
  • Downslope adjustment Use the lower knob.
Gys MULTIPEARL 201-4 — TIG EASY (VALVE TORCH) diagram (page 5)
Afb. 20
  • Post gas adjustment Keep button 3 pushed and at the same time use the upper knob to adjust the Post Gas.
Gys MULTIPEARL 201-4 — TIG EASY (VALVE TORCH) diagram (page 5)
Afb. 21

TIG EASY (VALVE TORCH)

  • Entering in TIG EASY mode (valve torch)

Keep button 2 pushed and at the same time turn the upper knob until "TIG EASY" is displayed.

Gys MULTIPEARL 201-4 — TIG EASY (VALVE TORCH) diagram (page 5)
Afb. 22
  • Welding current adjustment Use the upper knob.
Gys MULTIPEARL 201-4 — TIG EASY (VALVE TORCH) diagram (page 5)
Afb. 23

TIG LIFT WELDING

DC TIG welding requires the use of gas (Argon). Connecting a valve torch will allow to manually adjust the supply of gas and connec- ting a EURO torch will also offer capability to adjust downslope and post gas settings.

For TIG welding please follow the stages below :

TIG Lift Pro welding with a Euro torch TIG Lift EASY welding with a Valve torch

  • See connection page 4.
  • Connect the gas hose to the back of the machine and to the gas bottle regulator.
  • Adjust the gas flow on the gas bottle regulator.
  • To strike an arc touch the piece of metal to weld and press the torch trigger.
  • Downslope and Post-gas start automatically once the trigger is released. They can be adjusted on the device.
  • See connection page 4.
  • Connect the gas hose from the torch to the gas bottle regulator.
  • Adjust the gas flow on the gas bottle regulator and then open the torch valve.
  • Striking :

Touch the piece of metal to weld with the electrode

  • At the end of the weld :

Lift the electrode to between 2 to 5 mm from the metal.

Only stop the gas once the Tungsten electrode has cooled

down.

+ · +

Page 6 of the Gys MULTIPEARL 201-4 user manual — MAINTENANCE
Pagina 6 · klik om te vergroten
Pagina 6

Adjustable Downslope (Euro torch only) Time needed to shift from welding current to minimum current. Avoids cracks and craters at the end of welding. By default this fea- ture is set up at 0 sec.

Adjustable Post-Gas (Euro torch only) This parameter determines the time in which gas is released after the arc has stopped. It protects the weld pool and the electrode against oxidisation whilst the metal is cooling after welding.

Recommended settings / Electrode grinding

Gys MULTIPEARL 201-4 — DUTY CYCLE AND WELDING ENVIRONMENT diagram (page 6)
Afb. 24

wire (filler rod) ø Nozzle (mm) Flow (Argon L/min)

To optimise the welding process, it is recommended to grind the electrode prior to welding as described in the diagram below

DUTY CYCLE AND WELDING ENVIRONMENT

  • The welding unit described has a "constant current" output type. Its duty cycle following the norm EN60974-1 is indicated in the table below :
Gys MULTIPEARL 201-4 — DUTY CYCLE AND WELDING ENVIRONMENT diagram (page 6)
Afb. 25

X / 60974-1 @ 40°C (T cycle = 10 min) I max 60% (T cycle = 10 min) 100% (T cycle = 10 min)

MULTIPEARL 200.2 / 200.4 XL / 201.4 are Class A devices. It is designed to be used in an industrial or professional environment. In a different environment, it can be difficult to ensure electromagnetic compatibility, due to conducted disturbances as well as radiation. The device complies with the IEC 61000-3-12 standard.

THERMAL PROTECTION AND GUIDANCE

  • In thermal protection mode the device stops working. The overheating icon appears on the screen until the machine temperature is back within normal operating range.
  • Ensure the machine's vents are clear enabling air circulation.
  • Leave the device plugged in after welding to enable cooling. In general :
  • Respect the basic rules of welding.
  • Ensure the air circulation is good.
  • Do not work in a wet area.

MAINTENANCE

  • Maintenance must be only carried out by a qualified person.
  • Turn off the machine then unplug it from the mains. Wait until the fan has stopped before working on the device (DANGER High Voltage and Currents).
  • On a regular basis remove the side cover and clean the dust from the machine. Take this opportunity to have the electrical connections checked by a qualified person with an insulated tool.
  • Regularly check the condition of the power lead. If damaged, it will have to be replaced by the manufacturer, its’ after sales service or a qualified person.

L=2,5xd

Page 7 of the Gys MULTIPEARL 201-4 user manual — MIG/MAG
Pagina 7 · klik om te vergroten
Pagina 7

Safety

Arc welding can be dangerous and can cause serious and even fatal injuries. Protect yourself and others. Ensure the following safety precautions are taken :

Arc radiation: Protect yourself with a helmet fitted with filters in compliance with EN169 or EN 379.

Rain, steam, damp: Use your welding unit in a clean/dry environment (pollution factor ≤ 3), on a flat surface, and more than one meter from the welding work-piece. Do not use in rain or snow.

Electric choc: This device must only be used with an earthed power supply, single-phase or three- phase depending on model. Do not touch the parts under high voltage. Check that the power supply is suitable for this unit.

Falls: Do not place/carry the unit over people or objects.

Burns: Wear protective (fire-proof) clothing (cotton, overalls or jeans). Wear protective gloves and a fire-proof apron. Ensure other people keep a safe distance from the work area and do not look directly at the welding arc. Protect others by installing fire-proof protection walls.

Fire risks: Remove all flammable products from the work area. Do not work in presence of flammable gases.

Fumes: Do not inhale welding gases and fumes. Use the device in a well ventilated environment, with artificial extraction if welding indoors.

Additional Precautions: Any welding operation undertaken in - rooms where there is an increased risk of electric shocks, - Poorly ventilated rooms, - In the presence of flammable or explosive material, Use should always be approved by a «responsible expert», and made in presence of people trained to intervene in case of emergency. Technical protection as described in the Technical Specification CEI/IEC 62081 must be implemented. Welding in raised positions should not be undertaken, except in case of safety platforms use.

People wearing Pacemakers are advised not to use this machine, however if necessary, please seek medical advice prior to use. Do not use the welding unit to unfreeze pipes. Handle gas bottles with care - there is increased danger if the bottle or its valve are damaged.

TROUBLESHOOTING

SYMPTOMS POSSIBLE CAUSES REMEDIES

The welding wire speed is not constant. Cracklings block up the opening. Clean out the contact batch or change it and replace the anti-adherence product. Ref.041806

Control the roller pressure or replace it. Wire diameter non-consonant with roller. Covering Wire guide in the torch non-consonant.

The wire skids in the rollers.

MIG/MAG

The unwinding motor doesn't operate.

Reel or roller brake too tight. Release the brake and rollers.

Electrical supply problem. Check that the running button is on the position on.

Bad wire unwinding. Covering wire guide dirty or damaged. Clean or replace

Reel brake too tight Release the brake

Page 8 of the Gys MULTIPEARL 201-4 user manual — TIG
Pagina 8 · klik om te vergroten
Pagina 8

SYMPTOMS POSSIBLE CAUSES REMEDIES

Bad connection to the main supply. See the branch connection and look if the plug is fed by 3 phases.

Bad earth connection. Control the earth cable (connection and clamp condition).

Power contactor inoperative. Control the torch trigger.

Covering wire guide crushed. Check the covering and torch body.

The wire rubs down after the rollers.

Locking of the wire in the torch Clean or replace.

No capillary tube. Check the presence of capillary tube.

Wire speed too fast Reduce the wire speed

The welding cord is porous The gas flow rate is not sufficient. Adjusting flow range 15 to 20 L / min. Clean the working metal.

Gas bottle empty. Replace it.

Gas quality non-satisfying. Replace it.

Air flow or wind influence. Avert air blast, protect welding area.

Gas nozzle too full. Clean or replace the gas nozzle.

Bad wire quality. Use adapted WIRE for MIG-MAG welding.

Surface to weld in bad condtion. (rust, etc, ...) Clean the working parts before welding.

Arc voltage too low or too high. See welding settings.

Very important flashing particules.

Bad earth connection. Check and place the earth cable to have a better connection.

Protecting gas insufficient. Adjust the gas flow.

See if the gas coupling beside the engine is well connected. Check the flowmeter and the solenoid valves.

No gas at the torch output. Bad gas connection.

The machine does not deliver any current and the thermal overload indicator lamp lights up.

The welder thermal protection has turned on.

Wait for the end of the cooling time, around 2 minutes. The indicator lamp turns off.

The display is on but the device does not deliver any current.

The cable of the earth clamp or electrode holder is not connected to the welder. Check the connections.

If, when the unit is on and you put your hand on the welding unit’s body, you feel tingling sensation.

The welding unit is not correctly connected to the earth.

Check the plug and the earth of your electrical network.

The display is on but the device does not deliver any current.

The cable of the earth clamp or electrode holder is not connected to the welder. Check the connections.

The input voltage is outside of the range (230V + 15% for single phase or 400V + 15% for 3-phase). Have the electrical installation checked.

When starting up, the display indicates

Use a tungsten electrode with the adequate size

Default coming from the tungsten electrode

Use a well prepared tungsten electrode

Too important gas flow rate Reduce gas flow rate

TIG

Welding zone Protect welding zone against air flows

The tungsten electrode gets oxidised and tern at the end of welding.

Default coming from post-gas or the gas has been stopped prematurely.

Check and tighten all gas connections. Wait until the electrode cools down before stopping the gas.

The electrode melts Polarity error Check that the earth clamp is really connected to +

No welding current · In general · Instable arc

Probleemoplossing

Probleemoplossing

Veelvoorkomende problemen, mogelijke oorzaken en oplossingen.

ProbleemMogelijke oorzaakOplossing
No welding currentBad connection to the main supply. p.8
No welding currentBad earth connection. p.8
No welding currentPower contactor inoperative. p.8
The wire rubs down after the rollers.Covering wire guide crushed. p.8
The wire rubs down after the rollers.Locking of the wire in the torch p.8
The wire rubs down after the rollers.No capillary tube. p.8
The wire rubs down after the rollers.Wire speed too fast p.8
The welding cord is porousThe gas flow rate is not sufficient. p.8
The welding cord is porousGas bottle empty. p.8
The welding cord is porousGas quality non-satisfying. p.8
The welding cord is porousAir flow or wind influence. p.8
The welding cord is porousGas nozzle too full. p.8
The welding cord is porousBad wire quality. p.8
The welding cord is porousSurface to weld in bad condtion. (rust, etc, ...) p.8
Very important flashing particules.Arc voltage too low or too high. p.8
Very important flashing particules.Bad earth connection. p.8
Very important flashing particules.Protecting gas insufficient. p.8
No gas at the torch output.Bad gas connection. p.8
The machine does not deliver any current and the thermal overload indicator lamp lights up.The welder thermal protection has turned on. p.8
The display is on but the device does not deliver any current.The cable of the earth clamp or electrode holder is not connected to the welder. p.8
If, when the unit is on and you put your hand on the welding unit’s body, you feel tingling sensation.The welding unit is not correctly connected to the earth. p.8
When starting up, the display indicates .The input voltage is outside of the range (230V + 15% for single phase or 400V + 15% for 3-phase). p.8
Instable arcDefault coming from the tungsten electrode p.8
Instable arc p.8
Instable arcToo important gas flow rate p.8
The tungsten electrode gets oxidised and tern at the end of welding.Welding zone p.8
The tungsten electrode gets oxidised and tern at the end of welding.Default coming from post-gas or the gas has been stopped prematurely. p.8
The electrode meltsPolarity error p.8

Vraag stellen over de Gys MULTIPEARL 201-4

Eigenaren en ons team reageren doorgaans binnen een dag — en uw vraag helpt ook de volgende persoon.

Add your email to get notified when it’s answered — no spam, ever.

0 questions
Nog geen vragen over de Gys MULTIPEARL 201-4

Stel als eerste een vraag — andere eigenaren of ons team geven antwoord.

Origineel document

Gys MULTIPEARL 201-4 handleiding-pdf

71 pagina's·3.8 MB·Lasapparaat·PDF
Klik op een bovenstaande pagina om deze hier te openen
Pagina 1 / …
100%
Pagina's laden…